Compaction Matters: Three Keys to Better Asphalt Patches

Temperature, lift thickness, and edges matter when you want an asphalt patch to last.

For asphalt maintenance contractors, patching is one of those services that can look simple from the outside. Remove the failed material, put hot mix back in, compact it, and move on. However, anyone who has done enough patching knows there is a big difference between a patch that looks good when you leave the job and one that still looks good years later.

Whether you are performing a traditional remove-and-replace hot-mix patch or using an infrared heater to repair existing asphalt, compaction is one of the biggest factors determining the life of that repair. With more than two decades of asphalt maintenance experience with Wis-Coat, I can honestly tell you, I have had both versions. Education was the main thing that helped our patches get better.

Most maintenance contractors aren't showing up with a full-size paving train. We are working with plate compactors or compact ride-on rollers. That makes getting the fundamentals right even more important.

Here are three things to consider when trying to get the best possible compaction from your asphalt repairs as an asphalt maintenance contractor.

1. Temperature Is Your Working Window

Hot mix doesn't wait for you.

As asphalt cools, it becomes increasingly difficult to achieve proper density. That means your compaction process needs to be planned before the mix hits the patch, not figured out as you go.

Have your plate compactor or roller ready, fueled and positioned before placing the material. Once the mix is down, get it leveled and begin compaction while it is still workable.

The same principle applies to infrared repairs. After heating and scarifying the existing pavement, don't waste the temperature you just worked to create. Add rejuvenator or supplemental mix as required, properly blend and grade the repair, and get to compaction.

Weather matters, too. Cold pavement, wind and lower ambient temperatures can shorten your available compaction window considerably. So, plan on a warmer day, if you can.

We use a dump trailer at Wis-Coat and keep the mix double tarped once it is in the trailer. We haven’t insulated ours yet with foam and wood, but if we were going a long distance or need it to be hot longer, we would have to.

The hotter and more workable the material is when compaction begins, the better opportunity you have to achieve density (Compaction Rating).

2. Control Your Lift Thickness

One of the easiest mistakes to make is trying to compact too much asphalt at once.

A plate compactor or small roller only delivers so much compactive effort. If you place a deep patch in one thick lift, the surface may look tight while material deeper in the repair remains inadequately compacted.

For deeper repairs, build the patch in manageable lifts and compact each lift before adding the next.

Your lift thickness should make sense for the mix being used and the compaction equipment available. The goal isn't simply getting the material flat, it is getting compactive effort through the entire lift.

This is especially important for maintenance contractors because our equipment is smaller. Don't ask a plate compactor to accomplish what would normally require much heavier equipment. Rent the roller if you have to.

3. Pay Attention to the Edges

The center of the patch usually isn't where the trouble starts.

It's the edges.

Poorly compacted joints allow water intrusion and create an opportunity for the repair to begin separating from the surrounding pavement. Once water gets into that joint, freeze-thaw cycles and traffic can quickly accelerate failure.

Make deliberate passes along the perimeter of the repair. On hot-mix remove-and-replace patches, make sure the new material is properly consolidated against the existing pavement. With infrared repairs, focus on creating a tight transition between the repaired material and the surrounding asphalt.

Don't judge compaction only by how smooth the patch looks.

Temperature, lift thickness and edge compaction are three simple details that can separate a temporary patch from a professional asphalt repair.

For maintenance contractors, that's ultimately what the customer is paying for, not just black asphalt in a hole, but a repair designed to last.

These are a few things that have helped me with getting better results from my patches. I know there are other keys and tips to help even more, please feel free to reach out to me and let me know which ones I didn’t mention here, that have helped you.